AU Helps Improve Efficiency for Victor Insulators

November 8, 2012
/ Print / Reprints /
ShareMore
/ Text Size+

Alfred University (AU) recently announced it has helped Victor Insulators to improve its manufacturing efficiency. Because of AU’s work, Victor Insulators, a producer of electrical porcelain insulators in Victor, N.Y., can now machine a greater range of its existing products at an earlier point in the manufacturing process, according to William Carty, a professor of ceramic engineering at the Kazuo Inamori School of Engineering at Alfred University.

“We improved the manufacturing efficiency by machining [more products] in the wet state,” Carty said. “This manufacturing efficiency leads to better yields.”

“I am extremely proud of the fact that the ceramic engineering expertise of my Alfred University colleagues such as Dr. Carty can still make a significant impact in an industry that would generally be regarded as mature with little room for innovation,” said Matthew Hall, associate professor of biomaterials and glass science, as well as director of the New York State Center for Advanced Ceramic Technology (CACT).

The ability to machine the clay part earlier leads to fewer manufacturing losses because of product defects. “When machining dry green bodies, there is a greater rate of failure,” Carty said. 

Carty was reportedly able to increase the number of products machinable in the wet state by helping Victor Insulators adjust its chemistry during the mixing process.

For additional information, visit http://engineering.alfred.edu.

Did you enjoy this article? Click here to subscribe to Ceramic Industry Magazine.

You must login or register in order to post a comment.

Multimedia

Videos

Image Galleries

June 2014 Issue Highlights

Our June 2014 issue is now available!

Podcasts

Manufacturing Day 2014

Manufacturing Day organizers share their insights with Managing Editor Kelsey Seidler.

More Podcasts

Ceramic Industry Magazine

CI October 2014 cover

2014 October

Materials advances, refractories and renewable energy - oh, my! Check out our October issue today!

Table Of Contents Subscribe

Personal Smartphones

Do you use your personal smartphone or other device to complete tasks for your job?
View Results Poll Archive

THE CERAMIC INDUSTRY STORE

M:\General Shared\__AEC Store Katie Z\AEC Store\Images\Ceramics Industry\handbook of advanced ceramics.gif
Handbook of Advanced Ceramics Machining

Ceramics, with their unique properties and diverse applications, hold the potential to revolutionize many industries, including automotive and semiconductors.

More Products

Clear Seas Research

Clear Seas ResearchWith access to over one million professionals and more than 60 industry-specific publications,Clear Seas Research offers relevant insights from those who know your industry best. Let us customize a market research solution that exceeds your marketing goals.

STAY CONNECTED

facebook_40px twitter_40px  youtube_40pxlinkedin_40google+ icon 40px

Directories

CI Data Book July 2012

Ceramic Industry's Directories including Components, Equipment Digest, Services, Data Book & Buyers Guide, Materials Handbook and much more!