Ceramic Industry News / Refractories

RHI Opens Largest Raw Material Fusion Plant Outside of China

RHI recently announced it has built one of the largest fusion plants for magnesia raw materials for more than €75 million (~ $95 million) in Norway.

In this fusion plant, magnesia obtained from sea water is reportedly converted to fused magnesia, a high-grade refractory raw material, at temperatures about 2,800°F. With a capacity of approximately 85,000 tons per year, the plant is one of the largest worldwide. Some 120 employees will work at the plant in full operation.

“We are increasing self-supply with magnesia raw materials, which are very important for the refractories industry, to 80% and thus continue to consistently pursue our strategy of backward integration,” said Franz Struzl, CEO. “With this new plant, we will be completely independent from Asian fused magnesia imports. And we are shortening delivery routes to the European RHI sites.”

“The Porsgrunn location offers several advantages, including the infrastructure, the support of local politics and the energy costs in Norway,” said Roger Gravdal, plant manager. “In addition, we have decades of experience, which gives us a very good command of the complex process of obtaining magnesia from seawater. The construction of the fusion plant is one of the largest onshore investments in Norway in five years and is planned as a long-term investment.”

For additional information, visit www.rhi-ag.com

Did you enjoy this article? Click here to subscribe to Ceramic Industry Magazine.

You must login or register in order to post a comment.

Multimedia

Videos

Image Galleries

November 2014 Issue Highlights

Our November 2014 issue is now available! Posted: March 31, 2015.

Podcasts

Ceramics Expo podcast
Editor Susan Sutton discusses the upcoming Ceramics Expo with event director Adam Moore.
More Podcasts

Ceramic Industry Magazine

CI April 2015 edition

2015 April

You'll want to check out our continuing coverage of the inaugural Ceramics Expo event, plus articles on dental ceramics, glass coatings, refractories, and more!

Table Of Contents Subscribe

Daily News

We know where you find the latest ceramic industry news (ahem), but where do you catch up on the rest of your daily news?
View Results Poll Archive

THE CERAMIC INDUSTRY STORE

M:\General Shared\__AEC Store Katie Z\AEC Store\Images\Ceramics Industry\handbook of advanced ceramics.gif
Handbook of Advanced Ceramics Machining

Ceramics, with their unique properties and diverse applications, hold the potential to revolutionize many industries, including automotive and semiconductors.

More Products

Clear Seas Research

Clear Seas ResearchWith access to over one million professionals and more than 60 industry-specific publications,Clear Seas Research offers relevant insights from those who know your industry best. Let us customize a market research solution that exceeds your marketing goals.

STAY CONNECTED

facebook_40px twitter_40px  youtube_40pxlinkedin_40google+ icon 40px

Directories

CI Data Book July 2012

Ceramic Industry's Directories including Components, Equipment Digest, Services, Data Book & Buyers Guide, Materials Handbook and much more!