PPG Fiber Glass JV Starts Fourth Furnace in China

PPG Industries recently announced that PFG Fiber Glass (Kunshan) Co. Ltd., its joint venture in Kunshan, China, with Nan Ya Plastics Corp., has started a fourth furnace. With 38,000 metric tons of annual capacity, the additional furnace is expected to serve the expanding Asian electronics industries.

“This furnace features innovative, state-of-the-art technology,” said Terry Fry, general manager of global electronics for PPG and the company’s regional fiber glass business. “The technological advancements of its manufacturing operation enable us to maximize process efficiency while saving energy and reducing emissions.”

“Through our collaboration with Nan Ya, we have enabled PFG Fiber Glass (Kunshan) Co. Ltd. to maintain its position as the leader in the manufacture of fiber glass yarns for the electronics industry,” said Tom Kerr, PPG’s vice president for fiber glass. “We remain committed to our partners in Asia and to supporting the global fiber glass industry, its markets, and its customers.”

For additional information, visit www.ppg.com or www.npcusa.com.

Did you enjoy this article? Click here to subscribe to Ceramic Industry Magazine.

You must login or register in order to post a comment.

Multimedia

Videos

Podcasts

Thermal Processing Optimization: Using Advanced Rotary Tube Internals

Mike Maggio of Harper International discusses rotary tube internals with Susan Sutton, editor-in-chief.

More Podcasts

THE MAGAZINE

Ceramic Industry Magazine

CI May 2013 cover

2013 May

The 2013 May Ceramic Industry includes articles on treating heat like light, recycling, solar energy, and more. Check it out today!

Table Of Contents Subscribe

THE CERAMIC INDUSTRY STORE

M:\General Shared\__AEC Store Katie Z\AEC Store\Images\Ceramics Industry\handbook of advanced ceramics.gif
Handbook of Advanced Ceramics Machining

Ceramics, with their unique properties and diverse applications, hold the potential to revolutionize many industries, including automotive and semiconductors.

More Products

Clear Seas Research

Clear Seas ResearchWith access to over one million professionals and more than 60 industry-specific publications,Clear Seas Research offers relevant insights from those who know your industry best. Let us customize a market research solution that exceeds your marketing goals.

Directories

0711ci_cover.gif

Ceramic Industry's Directories including Components, Equipment Digest, Services, Data Book & Buyers Guide, Materials Handbook and much more!

STAY CONNECTED

facebook_40px twitter_40px  youtube_40pxlinkedin_40