Total BIPV System Capacity to Quintuple by 2017

January 8, 2013
/ Print / Reprints /
ShareMore
/ Text Size+

Both the building industry, which is still plagued by low housing starts and new builds, and the global solar industry, which is facing severe reductions in financial subsidies in key markets, have been under stress in recent years. The emergent market for building integrated photovoltaics (BIPV) offers a new way to develop revenue streams for these two industries.

According to a recent report from Pike Research, the total capacity of BIPV systems worldwide will grow from just over 400 MW in 2012 to 2,250 MW in 2017, a more than five-fold increase. The annual value of the BIPV market is expected to quadruple over the next five years, growing from $606 million in 2012 to more than $2.4 billion in 2017, the study concludes.

“The growing availability of energy-efficient, flexible, and transparent solar materials is transforming the way that architects and building engineers view, and use, photovoltaic systems,” said Kerry-Ann Adamson, research director. “In the future, BIPV will no longer be confined to spandrel or overhead applications. Rather, the entire building envelope will be able to put it to use, allowing the structure to produce its own power and feed additional power into the grid system.”

Going into 2013, the BIPV market is projected to open up more as it rebounds from the great solar depression and several long-term projects hit the market. An increasing number of players in the supply chain are working together to provide solutions for the entire building envelope. Among the most important next steps for the industry is the development of finished solar modules made by continuous production from PV rolls. Developing the ability to print the PV coating directly on to steel roof cladding will enable the modules to be cost-effectively produced in large volumes.

For additional information, visit www.pikeresearch.com.

Did you enjoy this article? Click here to subscribe to Ceramic Industry Magazine.

You must login or register in order to post a comment.

Multimedia

Videos

Image Galleries

In-Depth Features

These articles detail innovative advanced ceramic and glass materials and technologies.

Podcasts

Sapphire: An Extreme Performer

Ian Doggett of Goodfellow and CI Editor Susan Sutton discuss the benefits and opportunities provided by industrial sapphire.

More Podcasts

Ceramic Industry Magazine

CI April 2014 cover

2014 April

Our April issue features details on advanced materials such as ceramic matrix composites and piezoelectric ceramics, among many others. Be sure to check it out!

Table Of Contents Subscribe

THE CERAMIC INDUSTRY STORE

M:\General Shared\__AEC Store Katie Z\AEC Store\Images\Ceramics Industry\handbook of advanced ceramics.gif
Handbook of Advanced Ceramics Machining

Ceramics, with their unique properties and diverse applications, hold the potential to revolutionize many industries, including automotive and semiconductors.

More Products

Clear Seas Research

Clear Seas ResearchWith access to over one million professionals and more than 60 industry-specific publications,Clear Seas Research offers relevant insights from those who know your industry best. Let us customize a market research solution that exceeds your marketing goals.

Directories

CI Data Book July 2012

Ceramic Industry's Directories including Components, Equipment Digest, Services, Data Book & Buyers Guide, Materials Handbook and much more!

STAY CONNECTED

facebook_40px twitter_40px  youtube_40pxlinkedin_40