Global Alumina Production Rising

The shape and dynamics of the global bauxite and alumina industry are changing, according to a new report from Roskill. New alumina refining and bauxite production capacity are expected to boost supply over the next five years to meet the rising demand for aluminum, mainly from China, but also other growth areas such as the Middle East and India. The influence of China has changed the dynamics of the bauxite and alumina markets, and this will continue over the next five years.

World production of bauxite and alumina is growing. According to the report, Australia is the largest producer of bauxite, accounting for nearly 70 Mt in 2011; however, production in China, Indonesia and India has grown. Asia now accounts for 45% of global supply, compared with 16% a decade ago. This growth in non-captive bauxite production has led to sharp increases in shipped and traded bauxites, changing the dynamics of the marketplace.

Global alumina production increased from 80 to 96 Mt between 2007 and 2011, with most of the supply increase from China, which is now the largest producer. More refinery capacity is planned over the next three years, with another 14 Mt in China alone.  If it is all commissioned as scheduled, then the market will be oversupplied in the short term, until demand from the aluminum industry catches up, according to the report.

The growth in Chinese demand for bauxite has seen a significant rise in imports over the last five years, mainly from Indonesia, but also from Australia. Total Chinese imports have risen from 9 Mt in 2006 to 45 Mt in 2011. In early 2012, the Indonesian government shook the industry by announcing curbs on exports of unprocessed minerals, which is being phased in over the next two years. As a result, Indonesian bauxite exports to China fell to an estimated 28 Mt, down from 36 Mt in 2011. This will provide opportunities for other bauxite producers currently planning expansions and new projects in other countries to step in.

For additional information, visit www.roskill.com.

Did you enjoy this article? Click here to subscribe to Ceramic Industry Magazine.

You must login or register in order to post a comment.

Multimedia

Videos

Image Galleries

December 2014 Issue Highlights

Our December 2014 issue is now available! Posted: April 27, 2015.

Podcasts

Ceramics Expo podcast
Editor Susan Sutton discusses the upcoming Ceramics Expo with event director Adam Moore.
More Podcasts

Ceramic Industry Magazine

CI May 2015 cover

2015 May

Our May issue covers bulk batching, pneumatic conveyors, high-temperature furnaces and more! Be sure to check it out today.

Table Of Contents Subscribe

Daily News

We know where you find the latest ceramic industry news (ahem), but where do you catch up on the rest of your daily news?
View Results Poll Archive

THE CERAMIC INDUSTRY STORE

M:\General Shared\__AEC Store Katie Z\AEC Store\Images\Ceramics Industry\handbook of advanced ceramics.gif
Handbook of Advanced Ceramics Machining

Ceramics, with their unique properties and diverse applications, hold the potential to revolutionize many industries, including automotive and semiconductors.

More Products

Clear Seas Research

Clear Seas ResearchWith access to over one million professionals and more than 60 industry-specific publications,Clear Seas Research offers relevant insights from those who know your industry best. Let us customize a market research solution that exceeds your marketing goals.

STAY CONNECTED

facebook_40px twitter_40px  youtube_40pxlinkedin_40google+ icon 40px

Directories

CI Data Book July 2012

Ceramic Industry's Directories including Components, Equipment Digest, Services, Data Book & Buyers Guide, Materials Handbook and much more!