Owens Corning recently announced its inclusion in a strategic alliance with BASF and TenCate Advanced Composites. The goal of the alliance is to develop optimal solutions in thermoplastic composites for automotive mass production.

“There is a critical and growing need in the automotive industry to have lighter, stronger and more environmentally efficient products,” said Arnaud Genis, group president for Owens Corning. “Glass fiber solutions are not fully leveraged, and by combining the talent and resources of Owens Corning, BASF and TenCate—all industry leaders—we will be able to take significant weight out and find the optimum solutions for our customers quickly, and with the highest quality design and structure.”

In this strategic alliance, BASF contributes comprehensive knowledge in the production and formulation of thermoplastic resins, TenCate Advanced Composites brings its expertise in composites manufacturing, and Owens Corning brings the technology to develop superior and tailor-made fabrics and glass reinforcement solutions.

For additional information, visit www.owenscorning.com, www.tencate.com or www.basf.com.

Did you enjoy this article? Click here to subscribe to Ceramic Industry Magazine.

You must login or register in order to post a comment.

Multimedia

Videos

Image Galleries

December 2014 Issue Highlights

Our December 2014 issue is now available! Posted: April 27, 2015.

Podcasts

Ceramics Expo podcast
Editor Susan Sutton discusses the upcoming Ceramics Expo with event director Adam Moore.
More Podcasts

Ceramic Industry Magazine

CI May 2015 cover

2015 May

Our May issue covers bulk batching, pneumatic conveyors, high-temperature furnaces and more! Be sure to check it out today.

Table Of Contents Subscribe

Daily News

We know where you find the latest ceramic industry news (ahem), but where do you catch up on the rest of your daily news?
View Results Poll Archive

THE CERAMIC INDUSTRY STORE

M:\General Shared\__AEC Store Katie Z\AEC Store\Images\Ceramics Industry\handbook of advanced ceramics.gif
Handbook of Advanced Ceramics Machining

Ceramics, with their unique properties and diverse applications, hold the potential to revolutionize many industries, including automotive and semiconductors.

More Products

Clear Seas Research

Clear Seas ResearchWith access to over one million professionals and more than 60 industry-specific publications,Clear Seas Research offers relevant insights from those who know your industry best. Let us customize a market research solution that exceeds your marketing goals.

STAY CONNECTED

facebook_40px twitter_40px  youtube_40pxlinkedin_40google+ icon 40px

Directories

CI Data Book July 2012

Ceramic Industry's Directories including Components, Equipment Digest, Services, Data Book & Buyers Guide, Materials Handbook and much more!