Advanced Ceramics / Raw and Processed Materials

Flat Boron by the Numbers

Researchers calculate what it would take to make a new two-dimensional material.

June 3, 2013
Trans

It would be terrible if laboratories striving to grow graphene from carbon atoms kept winding up with big, pesky diamonds.

“That would be trouble, cleaning out the diamonds so you could do some real work,” said Rice University theoretical physicist Boris Yakobson, chuckling at the absurd image.

Yet something like that keeps happening to experimentalists working to grow two-dimensional boron. Boron atoms have a strong preference to clump into three-dimensional shapes rather than assemble into pristine single-atom sheets, like carbon does when it becomes graphene. And boron clumps aren’t nearly as sparkly.

Theoretical Possibilities

Yakobson and his Rice colleagues have made progress toward 2-D boron through theoretical work that suggests the most practical ways to make the material and put it to work. Earlier calculations by the group indicated 2-D boron would conduct electricity better than graphene.

Through first-principle calculations of the interaction of boron atoms with various substrates, the team came up with several possible paths experimentalists may take toward 2-D boron. Yakobson feels the work may point the way toward other useful two-dimensional materials.

The Rice team’s results appeared recently in the journal Angewandte Chemieinternational edition. Rice graduate student Yuanyue Liu and research scientist Evgeni Penev are co-authors of the paper.

Yakobson’s lab first reported in a Nano Letters paper last year that unlike graphene, 2-D boron rolled into a nanotube would always be metallic. Also unlike graphene, the atomic arrangement can change without changing the nature of the material. Instead of the steady rank-and-file of hexagons in a perfect graphene sheet, 2-D boron consists of triangles. But boron could have vacancies—missing atoms—without affecting its properties.

Practical Considerations

That’s the theory. The problem that remains is how to make the stuff.

“We are, perhaps, so close,” Penev said. “Here we have conceived a material that resembles graphene, but is always conductive no matter what form it takes. What we’re doing now is exploring different possibilities to connect our theories with reality.”

The best method, they calculated, might be to feed boron into a furnace with silver or gold substrates in a process called chemical vapor deposition, commonly used to make graphene. The substrate is important, Penev said, because the atoms have to spill onto the surface and stick, but not too strongly.

“You have to have a substrate that doesn’t want to dissolve boron,” he said. “On the other hand, you want a substrate that doesn’t bind too strongly. You should be able to detach the boron layer.”

Then, like graphene, these atom-thick boron sheets could be applied to other surfaces for testing and, ultimately, for use in applications.

The study also calculated methods for creating sheets via saturation of boron atoms on the surface of boride substrates, and the evaporation of metal atoms from metal borides that leaves just the target atoms in a sheet.

“There are a lot of reasons boron could be interesting,” said Liu, the paper’s first author. “Boron is carbon’s neighbor on the periodic table, with one less electron, which might bring in lots of new physics and chemistry, especially on the nanoscale. For example, 2-D boron is more conductive than graphene because of its unique electronic structure and atomic arrangement.

“In fact, comparing (boron) with graphene is very helpful,” he said. “The state-of-art synthesis methods for graphene provide us good templates to explore 2-D boron synthesis.”

Yakobson says he is thinking a step beyond the current work. “There are many groups, at Rice and elsewhere, working on 2-D boron,” he said. “To appreciate this work, you have to stand back and contrast it with graphene; in some sense, the synthesis of graphene is trivial.

“Why? Because graphene is a God-given material,” he said. “It forms at the global minimum (energy) for carbon atoms—they go there willingly. But boron is a different story. It does not have a planar form as a global minimum, which makes it a really subtle problem. The novelty in this work is that we’re trying to trick it into building a two-dimensional motif instead of three.”

Additional Possibilities

The search for 2-D materials with varying qualities is hot right now; another new paper from Rice on a hybrid graphene-hexagonal boron nitride shows the need for a 2-D semiconductor to complement the material’s conducting and insulating elements.

Yakobson hopes his study serves as a guideline for practical routes to other novel materials. “Now that there is a growing interest in a variety of 2-D materials, this may be a template,” he said.

Yakobson is Rice’s Karl F. Hasselmann Professor of Mechanical Engineering and Materials Science and professor of chemistry. The Department of Energy (DOE) supported the research. Computations were performed on the National Science Foundation-funded Data Analysis and Visualization Cyberinfrastructure at Rice, along with resources at the National Institute for Computational Sciences and the DOE’s National Energy Research Scientific Computing Center.


 For further details, visit www.rice.edu.  

 

Did you enjoy this article? Click here to subscribe to Ceramic Industry Magazine.

You must login or register in order to post a comment.

Multimedia

Videos

Image Galleries

November 2014 Issue Highlights

Our November 2014 issue is now available! Posted: March 31, 2015.

Podcasts

Ceramics Expo podcast
Editor Susan Sutton discusses the upcoming Ceramics Expo with event director Adam Moore.
More Podcasts

Ceramic Industry Magazine

CI April 2015 edition

2015 April

You'll want to check out our continuing coverage of the inaugural Ceramics Expo event, plus articles on dental ceramics, glass coatings, refractories, and more!

Table Of Contents Subscribe

Daily News

We know where you find the latest ceramic industry news (ahem), but where do you catch up on the rest of your daily news?
View Results Poll Archive

THE CERAMIC INDUSTRY STORE

M:\General Shared\__AEC Store Katie Z\AEC Store\Images\Ceramics Industry\handbook of advanced ceramics.gif
Handbook of Advanced Ceramics Machining

Ceramics, with their unique properties and diverse applications, hold the potential to revolutionize many industries, including automotive and semiconductors.

More Products

Clear Seas Research

Clear Seas ResearchWith access to over one million professionals and more than 60 industry-specific publications,Clear Seas Research offers relevant insights from those who know your industry best. Let us customize a market research solution that exceeds your marketing goals.

STAY CONNECTED

facebook_40px twitter_40px  youtube_40pxlinkedin_40google+ icon 40px

Directories

CI Data Book July 2012

Ceramic Industry's Directories including Components, Equipment Digest, Services, Data Book & Buyers Guide, Materials Handbook and much more!