This company’s Latrobe, Pa., site now manufactures ceramic insulators for industrial oil and gas burner igniters. These insulators can also reportedly be used for a range of other industrial applications such as fuses, precision electrical resistors and cartridge heaters.

A number of custom material formulations and blends are available that can be used for industrial igniters, including glazed and unglazed alumina and steatite. They can be produced with outer dimensions (OD) ranging from 0.050 to 2.5 in., and inner dimensions as small as 0.020 in. The igniters are available in lengths up to 12 in., and all the parts have counter bores and keyhole features.

For additional information, visit www.morganadvancedmaterials.com.

Did you enjoy this article? Click here to subscribe to Ceramic Industry Magazine.

You must login or register in order to post a comment.

Multimedia

Videos

Image Galleries

June 2014 Issue Highlights

Our June 2014 issue is now available!

Podcasts

Manufacturing Day 2014

Manufacturing Day organizers share their insights with Managing Editor Kelsey Seidler.

More Podcasts

Ceramic Industry Magazine

CI October 2014 cover

2014 October

Materials advances, refractories and renewable energy - oh, my! Check out our October issue today!

Table Of Contents Subscribe

THE CERAMIC INDUSTRY STORE

M:\General Shared\__AEC Store Katie Z\AEC Store\Images\Ceramics Industry\handbook of advanced ceramics.gif
Handbook of Advanced Ceramics Machining

Ceramics, with their unique properties and diverse applications, hold the potential to revolutionize many industries, including automotive and semiconductors.

More Products

Clear Seas Research

Clear Seas ResearchWith access to over one million professionals and more than 60 industry-specific publications,Clear Seas Research offers relevant insights from those who know your industry best. Let us customize a market research solution that exceeds your marketing goals.

Directories

CI Data Book July 2012

Ceramic Industry's Directories including Components, Equipment Digest, Services, Data Book & Buyers Guide, Materials Handbook and much more!

STAY CONNECTED

facebook_40px twitter_40px  youtube_40pxlinkedin_40google+ icon 40px