Ceramic Industry News / Decorating Ceramics / Whitewares

Sacmi Installs Digital Printer for Belarus-Based Tile Company

Tile manufacturer JSC Beryozastroymaterialy recently launched an investment plan that aims to raise product quality, introduce new designs, optimize materials use, reduce waste and improve logistics. The plan also includes a focus on the opportunities offered by digital decoration; therefore, the company chose a COLORA HD2 built by Intesa, the Sacmi Group company that specializes in digital printing and glazing solutions for ceramic tile.

Featuring five color bars, each with seven print heads, the COLORA HD2 can print any type of pattern at speeds of up to 48 m/min. Given the print width, which reaches 488 mm, the machine can also be used for large sizes and complex designs. The machine was installed and started up on a single-firing line that produces 1.5 million m2 of 400 x 400 and 300 x 300 tile per year.

Sacmi’s technicians provided JSC staff with support throughout installation and testing. Owned by the Ministry of Agricultural Construction, the company, based in Beryoza in the region of Brest (Belarus), thus completes another strategic stage of an investment plan involving an output that, taking into account double- and third-firing operations, exceeds 10 million m2 a year.

For additional information, visit www.sacmi.com.

Did you enjoy this article? Click here to subscribe to Ceramic Industry Magazine.

You must login or register in order to post a comment.

Multimedia

Videos

Image Galleries

October 2014 Issue Highlights

Our October 2014 issue is now available!

Posted: January 29, 2015

Podcasts

Ceramics Expo podcast
Editor Susan Sutton discusses the upcoming Ceramics Expo with event director Adam Moore.
More Podcasts

Ceramic Industry Magazine

CI March 2015 cover

2015 March

We're focusing on thermal processes and decorating in this issue. Check it out!

Table Of Contents Subscribe

Daily News

We know where you find the latest ceramic industry news (ahem), but where do you catch up on the rest of your daily news?
View Results Poll Archive

THE CERAMIC INDUSTRY STORE

M:\General Shared\__AEC Store Katie Z\AEC Store\Images\Ceramics Industry\handbook of advanced ceramics.gif
Handbook of Advanced Ceramics Machining

Ceramics, with their unique properties and diverse applications, hold the potential to revolutionize many industries, including automotive and semiconductors.

More Products

Clear Seas Research

Clear Seas ResearchWith access to over one million professionals and more than 60 industry-specific publications,Clear Seas Research offers relevant insights from those who know your industry best. Let us customize a market research solution that exceeds your marketing goals.

STAY CONNECTED

facebook_40px twitter_40px  youtube_40pxlinkedin_40google+ icon 40px

Directories

CI Data Book July 2012

Ceramic Industry's Directories including Components, Equipment Digest, Services, Data Book & Buyers Guide, Materials Handbook and much more!