New Products / Product Highlights

Aremco Products, Inc.: Machinable Ceramic

Aremco Products, Inc. has introduced AremcoloxTM 502-1100-UF, an advanced alumino-silicate machinable ceramic for producing reliable, low-cost brazing fixtures and a wide variety of industrial parts, such as electrical and thermal insulators, burner and combustion nozzles, and welding shields. The material demonstrates exceptional mechanical, electrical and thermal properties, including a compressive strength of 25 kpsi, dielectric strength of 100 volts per mil, and thermal conductivity of 9.0 Btu-in/hr-ft(2)-F. Its coefficient of thermal expansion is 2.5 in/in/F x 10(-6), making it ideal for thermal shock applications. Aremcolox 502-1100-UF can be machined easily using conventional tooling. After a simple firing procedure, it is fully dense and resistant to 2100F.

For additional information, call (845) 268-0039, fax (845) 268-0041, e-mail aremco@aremco.com or visit http://www.aremco.com.

Did you enjoy this article? Click here to subscribe to Ceramic Industry Magazine.

You must login or register in order to post a comment.

Multimedia

Videos

Podcasts

Thermal Processing Optimization: Using Advanced Rotary Tube Internals

Mike Maggio of Harper International discusses rotary tube internals with Susan Sutton, editor-in-chief.

More Podcasts

THE MAGAZINE

Ceramic Industry Magazine

CI May 2013 cover

2013 May

The 2013 May Ceramic Industry includes articles on treating heat like light, recycling, solar energy, and more. Check it out today!

Table Of Contents Subscribe

THE CERAMIC INDUSTRY STORE

M:\General Shared\__AEC Store Katie Z\AEC Store\Images\Ceramics Industry\handbook of advanced ceramics.gif
Handbook of Advanced Ceramics Machining

Ceramics, with their unique properties and diverse applications, hold the potential to revolutionize many industries, including automotive and semiconductors.

More Products

Clear Seas Research

Clear Seas ResearchWith access to over one million professionals and more than 60 industry-specific publications,Clear Seas Research offers relevant insights from those who know your industry best. Let us customize a market research solution that exceeds your marketing goals.

Directories

0711ci_cover.gif

Ceramic Industry's Directories including Components, Equipment Digest, Services, Data Book & Buyers Guide, Materials Handbook and much more!

STAY CONNECTED

facebook_40px twitter_40px  youtube_40pxlinkedin_40