Ceradyne Receives Record Body Armor Order (1/9/07)

January 9, 2007
/ Print / Reprints /
ShareMore
/ Text Size+

Ceradyne, Inc. recently received a $133 million delivery order for enhanced side ballistic inserts (ESBI) from the U.S. Army, Aberdeen Proving Ground, Md. This new delivery order, scheduled to be shipped April 2007 through November 2007, will be shipped against a larger indefinite delivery/indefinite quantity (ID/IQ) contract announced earlier. Ceradyne records as firm orders only delivery orders, such as the above, that have scheduled delivery dates.

“This delivery order is the largest single order ever received by Ceradyne,” said Dave Reed, Ceradyne president North American Operations. “Together with the $122.2 million in ESAPI and ESBI body armor orders announced last month, we have excellent visibility into 2007. We anticipate receiving additional orders early in 2007 for delivery in 2007.”

The company’s website is located at www.ceradyne.com.

Links

Did you enjoy this article? Click here to subscribe to Ceramic Industry Magazine.

You must login or register in order to post a comment.

Multimedia

Videos

Image Galleries

In-Depth Features

These articles detail innovative advanced ceramic and glass materials and technologies.

Podcasts

Sapphire: An Extreme Performer

Ian Doggett of Goodfellow and CI Editor Susan Sutton discuss the benefits and opportunities provided by industrial sapphire.

More Podcasts

THE MAGAZINE

Ceramic Industry Magazine

CI April 2014 cover

2014 April

Our April issue features details on advanced materials such as ceramic matrix composites and piezoelectric ceramics, among many others. Be sure to check it out!

Table Of Contents Subscribe

THE CERAMIC INDUSTRY STORE

M:\General Shared\__AEC Store Katie Z\AEC Store\Images\Ceramics Industry\handbook of advanced ceramics.gif
Handbook of Advanced Ceramics Machining

Ceramics, with their unique properties and diverse applications, hold the potential to revolutionize many industries, including automotive and semiconductors.

More Products

Clear Seas Research

Clear Seas ResearchWith access to over one million professionals and more than 60 industry-specific publications,Clear Seas Research offers relevant insights from those who know your industry best. Let us customize a market research solution that exceeds your marketing goals.

Directories

CI Data Book July 2012

Ceramic Industry's Directories including Components, Equipment Digest, Services, Data Book & Buyers Guide, Materials Handbook and much more!

STAY CONNECTED

facebook_40px twitter_40px  youtube_40pxlinkedin_40