Drying: Principles of Drying

Understanding the principles of drying will enable us to make informed decisions about the type of dryer we purchase for our facility.

A conventional tunnel dryer used for drying whitewares. Photo courtesy of Eisenmann Corp.
In this day of wonderful technological achievements and automatic devices for drying, it can be difficult to remember what it is we are trying to accomplish. We must not forget that the point of drying is simply to remove water from the ceramic without causing any damage. Of course, this process must be done both efficiently and economically.

No matter what kind of drying we do—whether basic air drying or sophisticated electronic drying—water can only leave the surface of the ceramic at a given rate. The real trick to drying is to use a method that removes the water from the inside of the ceramic as fast as that surface water is evaporated. To accomplish this process, we must first understand 1) the factors that control how quickly the water can leave the surface, and 2) the factors that control how quickly the water can move from the inside of the piece to the surface. Understanding these principles will then enable us to make informed decisions about the type of dryer we purchase for our facility.

A conventional tunnel dryer used in the brick industry. Photo courtesy of Harrop Industries Inc.

How Quickly Does Water Leave the Surface?

Water from the surface of a piece of ceramic cannot move into the surrounding air any faster than it would from a pool of standing water. Fortunately, that speed was determined for us at about the turn of the last century by Willis Carrier, the man who invented air conditioning. The heating, ventilating and air conditioning (HVAC) industry uses the following equation derived from Carrier’s work to establish the maximum rate of evaporation from a pool of water:

lb water/sq. ft. of surface area/hr = k(1+200/V)(W0–WRH)

where k is a constant for the particular situation (often taken as 0.192) and V is the perpendicular air velocity in feet per minute. Omega saturated (W0) is the partial pressure of water vapor in fully saturated air at the given temperature in inches mercury, and Omega relative humidity (WRH) is the percent of saturation as denoted by the percent relative humidity. These numbers are well known and are available in standard tables.1

The equation says that at a given air velocity and a given temperature, only so many pounds of water can be removed per hour for each square foot of exposed surface area. The means that no matter what we change inside the piece, the water can still only leave the surface at some fixed rate. However, at high temperatures or high air velocities, this rate can be quite high. In fact, even in an open manufacturing room with low humidity, the speed of surface drying is so fast that even a gentle air movement is enough to cause pieces to warp before they are put into a dryer. For this reason, many manufacturers cover their ware with plastic immediately after forming to avoid having it dry too quickly on one surface. Drying one surface faster than another will cause that surface to shrink faster than the other side. This shrinkage causes a difference in movement often seen as a warp or crack. (See “Understanding Shrinkage” sidebar.) Even a piece that looks fine after drying can have hairline cracks that may not be visible until after the piece is fired. This defect, often mistaken for firing cracks (preheating cracks), can be prevented by drying on all sides evenly and by drying the surface no faster than the surface water can be replaced from the inside of the piece.

A self-contained conventional dryer. Photo courtesy of Ceramic Services, Inc.

How Quickly Does Water Move to the Surface?

The answer to how fast water moves from the inside of a piece to the outside is very complicated. We know that a mix of materials with larger diameter capillaries will allow faster water movement than smaller diameter capillaries. We also know that warmer water has lower viscosity than cooler water, so it will effectively be “thinner” and move more easily through the capillaries, or pores, inside the ware. But how can these principles be applied to ensure perfect drying?

Raising the temperature of the inside of the piece will allow the water to move a little more quickly to the surface by lowering the viscosity of the water (i.e., the “thinner” water moves through the pores of the ware more easily). However, the temperature must be carefully controlled. If the water turns into steam, it might move from the surface more quickly, but the expansion of the water to steam could cause internal damage to the ware.

Of course, steam does not always harm a ceramic body. Some mixes are very “forgiving” and dry easily. In other formulations, adding grog to the body can enhance the drying process by enlarging the capillaries to allow the water to pass more easily from the inside to the outside of the ware. Any steam formed in these types of pieces can escape almost instantaneously without damaging the ware. In other cases, the green strength of the body is high enough that the expanding steam can be contained without harming the bond. However, these examples are all exceptions to the norm. The formation of steam during drying will damage most body formulations, and should therefore be avoided through carefully controlled drying whenever possible.

Heat can be applied to a drying ceramic to raise the temperature of the inside water and make it migrate to the surface more easily, but it must not be applied too soon in the drying process. If the ceramic is too wet, the water will be removed from the surface of the ware faster than it can migrate from the inside of the ware to the surface, as explained previously. On the other hand, a piece that does not contain much water going into the drying stage can be dried faster—with heat—and without much risk of damage. How much water a piece contains depends on its body formulation and on how it was formed. For example, dry pressed ware has very little water (approximately 5-6%) and can dry quite quickly. Ceramics that do not contain a lot of clay can also be safely dried faster than their clay-laden counterparts, which will shrink significantly during the drying process. (See “ Determining Water Content” sidebar.)

In any case, the secret to good drying is to drive the water from the center of the piece to the outside surface and then remove it as fast as it gets there—not simply to remove the water as fast as possible from the surface.

A hybrid RF/convection heating system. Photo courtesy of Radio Frequency Co., Inc.

Drying Methods

Once we understand how the drying process works, we will then be better equipped to choose the right type of dryer for our facility. Four basic drying methods are used in the ceramic industry:

  • Air drying or open drying
  • Air drying in a closed room
  • Drying in a conventional dryer
  • Microwave and radio frequency (RF) drying

Air drying or open drying is the most inconsistent form of drying and is mainly used by small facilities and studios. In this form of drying, products are placed on shelves in the manufacturing facility and allowed to air dry. In some cases, the products are set on the ground outside and allowed to dry in the sun. Aside from the great lengths of time that this drying process requires, many products are often damaged due to the inability to control drying conditions.

Many of the manufacturers that once air-dried their products have “upgraded” to a closed room reserved specifically for this purpose. In reality, a closed room provides little improvement over air drying. Although confining the products in one indoor room provides slightly more control over the climate, conditions are still largely unregulated, and numerous losses still result.

For many ceramic facilities, a conventional dryer provides sufficient speed and control to ensure thorough, efficient drying. The conventional dryer is either a stationary enclosed room or a continuously moving platform through an enclosed room, in which the speed and direction of the air can be controlled. In some cases, the dryer is nothing more than a series of heaters placed so that the product passes by them. In other cases, the dryer provides very large movements of air with a series of increasing temperatures, and many of today’s models offer programmable control over both the temperature and relative humidity of the air. (See “More About Conventional Dryers” sidebar.)

More recently, microwave and RF dryers have also been put into service. These dryers work by sending electromagnetic energy to the water molecules inside the ware. The ceramic is transparent to these waves of energy, so all of the water inside the piece is affected. Radio frequency dryers operate on a different frequency than microwave dryers and are able to evenly excite all of the water molecules throughout the ceramic, so that the water migrates from the inside to the outside at a more uniform rate. The factory space required for an RF dryer is often smaller than the space required for a conventional dryer. And since heating begins instantaneously throughout the product, the dwell time in an RF dryer is far less than in a conventional dryer. However, their smaller size also restricts the size of the ware that can be placed in the dryers, limiting them mainly to small components and glass fibers. There is also a danger that the pieces may heat too much and cause steam or expanding water vapor to harm the piece.

Selecting a Dryer

Which dryer you choose depends on your ware. Some manufacturers require several weeks to dry their ware. Others are able to dry their products completely in 48 hours using a modern conventional dryer, and many have achieved drying cycles of 24 hours or less.

For most ceramic products, superior drying results can be obtained in very short periods of time using judicial air movement, humidity control and temperatures below 120°F. The fastest drying time for a given piece depends on:

  • The moisture content of the piece (more moisture will take more time)
  • The size and shape of the finished ware (thinner ware dries faster, and smooth shapes dry faster than complex shapes)
  • The forming process used
  • How difficult the mix is to dry

Conventional drying with properly controlled air velocity, temperature and relative humidity can be very inexpensive and is fast enough for many operations. Because of several issues, including the relatively high energy costs involved, microwave and RF dryers are still practical for only a handful of applications, mostly in the high-tech arena. However, when speed is of the utmost importance and uniform drying is crucial, the benefits of these systems can easily offset the extra energy and purchasing costs.

A dryer is an investment that should benefit your plant over the long run. Evaluate your needs, and request test runs from potential suppliers. In the end, the dryer that works best with your product—and the supplier that best meets your needs—is the one you should choose.

Drying is an important part of any ceramic manufacturing process. Understanding how the drying stage works, and then choosing the best dryer for your facility and ware requirements, will go a long way toward ensuring a successful, problem-free manufacturing operation.

Editor's Note

For more information about drying, consider attending the Ceramic Manufacturers Association (CerMA) fall workshop, “Drying, Glazing and Firing.” The workshop will be held in Batavia, N.Y., September 13-14, 2001. For more information, contact CerMA at 1100-H Brandywine Blvd, PO Box 3388, Zanesville, OH 43702-3388; (740) 452-4541; fax (740) 452-2552; or e-mail cerma.info@offinger.com.

SIDEBAR: Understanding Shrinkage

Clay has an affinity for water, i.e., water will “cling” to the clay grain and may be rather difficult to separate from the clay. Not all products contain clay, however, so the study of drying must include insights into how the water leaves the compacted mass of ceramic, as well as how the water leaves the individual clay grains.

When any ceramic is very wet, with or without the presence of clay, the water leaves the surface very easily. As the ceramic becomes drier, the grains of material shrink together to fill the space occupied by that water. It is this shrinkage that brings the danger of damage to the ware during drying. If one side dries more than another and, hence, shrinks more than the other, the piece will either warp or crack. (If the ceramic is made of relatively coarse or non-plastic particles particles, enough space may exist between grains to allow the water to leave without any appreciable shrinkage.)

As the ceramic continues to dry it finally stops shrinking. However, the “safe point” is not reached until all the ceramic has stopped shrinking, including the inside.

Once all shrinkage has stopped, the temperature can be increased to speed the remaining drying. Adding heat lowers the viscosity of the entrapped water, allowing it to move more freely through the small spaces until the piece is completely dry.

SIDEBAR: Determining Water Content

The amount of water in a piece of ware will affect the success of the drying process. In most cases, the manufacturer’s knowledge of the water present in the original body formulation is sufficient to determine the best drying process. However, scientific methods of determining the water content of a ceramic body also exist.

To determine water content using a non-destructive method, weigh the piece at the outset and continue drying until the piece stops losing weight. Subtract the light weight from the heavy weight, and divide by the light weight to determine the percentage of water in the piece at the start of the drying process. This method is cumbersome and generally cannot be used to provide immediate improvements in the production process because of the time required to complete the tests. However, if the dryer being used is sufficiently modern and repeatable, the final test results can be used to improve the overall drying process.

A faster but destructive method of determining water content involves placing pieces of a known size and weight into a dryer and pulling them out at predetermined intervals. Weigh the pieces, then grind them to a powder and place the powder under a heat lamp mounted on a scale. The scale will indicate the percentage of water present in the powder and therefore in the ceramic body.

SIDEBAR: More About Conventional Dryers

Air/airless dryers, infra red dryers, jet dryers, steam dryers, gas-fired dryers and waste heat dryers are all various types of conventional dryers. Each type merely emphasizes one of the three forms of drying (air speed, temperature or humidity) or indicates the energy source (gas, waste heat, steam, etc.).

Other types of “conventional” dryers include vacuum dryers, which use a vacuum in conjunction with a conventional drying system, and dielectric dryers, which are similar to microwave or RF dryers but operate at lower frequencies.

Some manufacturers also use their kilns as dryers; however, this practice is not recommended. A kiln costs a lot more to operate than a dryer and can cause a great deal of product losses due to inefficient/ineffective drying.

Did you enjoy this article? Click here to subscribe to Ceramic Industry Magazine.

Cameron Harman Jr. is a kiln expert from Ceramic Services, Inc., Bensalem, Pa. If you have drying or firing questions that you would like to have answered, send them to Cameron Harman Jr., c/o Ceramic Industry, Business News Publishing Co., 755 West Big Beaver Road, Suite 1000, Troy, MI 48084, fax (248) 244-1294; or contact Cameron directly at (215) 245-4040, fax (215) 638-1812. Look for Cameron’s answers to your questions in upcoming issues of Ceramic Industry magazine.

Recent Articles by Cameron Harman Jr.

You must login or register in order to post a comment.

Multimedia

Videos

Podcasts

Thermal Processing Optimization: Using Advanced Rotary Tube Internals

Mike Maggio of Harper International discusses rotary tube internals with Susan Sutton, editor-in-chief.

More Podcasts

THE MAGAZINE

Ceramic Industry Magazine

CI May 2013 cover

2013 May

The 2013 May Ceramic Industry includes articles on treating heat like light, recycling, solar energy, and more. Check it out today!

Table Of Contents Subscribe

THE CERAMIC INDUSTRY STORE

M:\General Shared\__AEC Store Katie Z\AEC Store\Images\Ceramics Industry\handbook of advanced ceramics.gif
Handbook of Advanced Ceramics Machining

Ceramics, with their unique properties and diverse applications, hold the potential to revolutionize many industries, including automotive and semiconductors.

More Products

Clear Seas Research

Clear Seas ResearchWith access to over one million professionals and more than 60 industry-specific publications,Clear Seas Research offers relevant insights from those who know your industry best. Let us customize a market research solution that exceeds your marketing goals.

Directories

0711ci_cover.gif

Ceramic Industry's Directories including Components, Equipment Digest, Services, Data Book & Buyers Guide, Materials Handbook and much more!

STAY CONNECTED

facebook_40px twitter_40px  youtube_40pxlinkedin_40