Dyson Ceramics Systems: Dylite Cordierite Material

Dyson Ceramic Systems has introduced Dylite, a new cordierite material that is almost half the weight of standard cordierite. The new material gives kiln furniture users the potential to obtain refractory weight savings of up to 50%, achieve faster firing cycles and reduce energy consumption substantially. Developed by Dyson over a period of three years, Dylite offers many additional benefits to refractory users. Thermal shock resistance is improved over standard cordierite, giving longer refractory life, and the new material's lower specific heat capacity enables quicker heating and cooling. Rapid firing is therefore a real possibility with Dylite, giving the opportunity to increase kiln speed and throughput. Refractory coating is also improved. The new material's high porosity enables cover wash to be more easily absorbed and adhere to the refractory, giving an improved protective coating.

For additional information, call (44) 1782 711511, fax (44) 1782 717078, e-mail enq@dyson-ceramic-systems.com or visit http://www.dyson-ceramic-systems.com.

Did you enjoy this article? Click here to subscribe to Ceramic Industry Magazine.

You must login or register in order to post a comment.

Multimedia

Videos

Podcasts

Thermal Processing Optimization: Using Advanced Rotary Tube Internals

Mike Maggio of Harper International discusses rotary tube internals with Susan Sutton, editor-in-chief.

More Podcasts

THE MAGAZINE

Ceramic Industry Magazine

CI May 2013 cover

2013 May

The 2013 May Ceramic Industry includes articles on treating heat like light, recycling, solar energy, and more. Check it out today!

Table Of Contents Subscribe

THE CERAMIC INDUSTRY STORE

M:\General Shared\__AEC Store Katie Z\AEC Store\Images\Ceramics Industry\handbook of advanced ceramics.gif
Handbook of Advanced Ceramics Machining

Ceramics, with their unique properties and diverse applications, hold the potential to revolutionize many industries, including automotive and semiconductors.

More Products

Clear Seas Research

Clear Seas ResearchWith access to over one million professionals and more than 60 industry-specific publications,Clear Seas Research offers relevant insights from those who know your industry best. Let us customize a market research solution that exceeds your marketing goals.

Directories

0711ci_cover.gif

Ceramic Industry's Directories including Components, Equipment Digest, Services, Data Book & Buyers Guide, Materials Handbook and much more!

STAY CONNECTED

facebook_40px twitter_40px  youtube_40pxlinkedin_40