GEO2 Technologies Inc.: Silicon Carbide Substrate

GEO2 Technologies Inc. has introduced a new silicon carbide (SiC) substrate for diesel particulate filtering. GEO2’s patented microstructure is poised to drive the next wave of high-temperature filter innovation, effectively removing 99% of pollutants from diesel exhaust while achieving better fuel economy, emissions control and enhanced engine performance.

The new substrate simultaneously achieves high porosity and high strength while delivering lower back-pressure and high trapping efficiency. Also, unlike other SiC products, GEO2 filters are based on a cross-linked microstructure (CLM) that effectively reduces the size, weight and cost of emissions control systems.

“Today, the need for clean transportation technology is critical, given the growing number of health and environmental issues associated with fossil fuels,” said Bilal Zuberi, vice president and co-founder, GEO2 Technologies. “By innovating solutions such as the new cross-linked microstructure SiC diesel particulate filter, we can offer auto manufacturers an affordable means of controlling toxic particulate and CO2 emissions while preserving all the benefits of diesel fuel, including better gas mileage and improved vehicle performance.”

For more information, visit www.geo2tech.com.

Links

Did you enjoy this article? Click here to subscribe to Ceramic Industry Magazine.

You must login or register in order to post a comment.

Multimedia

Videos

Podcasts

Thermal Processing Optimization: Using Advanced Rotary Tube Internals

Mike Maggio of Harper International discusses rotary tube internals with Susan Sutton, editor-in-chief.

More Podcasts

THE MAGAZINE

Ceramic Industry Magazine

CI May 2013 cover

2013 May

The 2013 May Ceramic Industry includes articles on treating heat like light, recycling, solar energy, and more. Check it out today!

Table Of Contents Subscribe

THE CERAMIC INDUSTRY STORE

M:\General Shared\__AEC Store Katie Z\AEC Store\Images\Ceramics Industry\handbook of advanced ceramics.gif
Handbook of Advanced Ceramics Machining

Ceramics, with their unique properties and diverse applications, hold the potential to revolutionize many industries, including automotive and semiconductors.

More Products

Clear Seas Research

Clear Seas ResearchWith access to over one million professionals and more than 60 industry-specific publications,Clear Seas Research offers relevant insights from those who know your industry best. Let us customize a market research solution that exceeds your marketing goals.

Directories

0711ci_cover.gif

Ceramic Industry's Directories including Components, Equipment Digest, Services, Data Book & Buyers Guide, Materials Handbook and much more!

STAY CONNECTED

facebook_40px twitter_40px  youtube_40pxlinkedin_40