Molybdenum is also useful as an alloying agent in certain grades of steel to produce very hard materials used in cutting tools and to protect surfaces subject to heavy wear. Goodfellow offers molybdenum in a number of forms, including microfoil, foil, sputtering target, mesh, wire, insulated wire, rod, tube, powder, lump and single crystal.
Details are available at www.goodfellow.com.