Ceramic Industry News

Int'l News: New Cutting Insert Features High Wear Resistance

SPK Cutting Tools, a division of CeramTec AG, has extended its range of indexable inserts to include the coated Cermet SC 7035 and the -MQ chip breaker. With its TiAlN coating on a tough Cermet substrate, the new SC 7035 grade is said to possess outstanding wear resistance and is suitable for a broad range of applications from semi-roughing to finishing. Applications embrace the turning of case-hardening and heat-treatment steels, as well as supplementary uses on stainless steels and cast iron. Extensive tests have demonstrated superb quality in terms of surface finish, dimensional and shape tolerances when turning small- to medium-stress cross-sections, the company reports.

The new coated cutting material (ISO HC-P15) is suitable for finish-turning, in one step at moderate feed rates, workpieces with small to medium allowances of up to around 1.5 mm. These are ideal near-net shape preconditions. SC 7035 largely overlaps the application range of uncoated Cermets while reaching out further toward greater wear resistance. With the possibility of dry machining and no need for lubricants while cutting, advantages are reported to be both ecological and economical.

Available in all the important basic insert geometries, the -MQ chip breaker provides an addition to the existing range of chip breakers for negative insert geometries -SP, -MB, and -MK, and ensures reliable chip control and automation-compatible chip breaking for feeds of 0.10 to 0.30 mm and cutting depths of 0.4 to 1.5 mm.

Did you enjoy this article? Click here to subscribe to Ceramic Industry Magazine.

You must login or register in order to post a comment.

Multimedia

Videos

Podcasts

Thermal Processing Optimization: Using Advanced Rotary Tube Internals

Mike Maggio of Harper International discusses rotary tube internals with Susan Sutton, editor-in-chief.

More Podcasts

THE MAGAZINE

Ceramic Industry Magazine

CI May 2013 cover

2013 May

The 2013 May Ceramic Industry includes articles on treating heat like light, recycling, solar energy, and more. Check it out today!

Table Of Contents Subscribe

THE CERAMIC INDUSTRY STORE

M:\General Shared\__AEC Store Katie Z\AEC Store\Images\Ceramics Industry\handbook of advanced ceramics.gif
Handbook of Advanced Ceramics Machining

Ceramics, with their unique properties and diverse applications, hold the potential to revolutionize many industries, including automotive and semiconductors.

More Products

Clear Seas Research

Clear Seas ResearchWith access to over one million professionals and more than 60 industry-specific publications,Clear Seas Research offers relevant insights from those who know your industry best. Let us customize a market research solution that exceeds your marketing goals.

Directories

0711ci_cover.gif

Ceramic Industry's Directories including Components, Equipment Digest, Services, Data Book & Buyers Guide, Materials Handbook and much more!

STAY CONNECTED

facebook_40px twitter_40px  youtube_40pxlinkedin_40