Columns / Kiln Connection

KILN CONNECTION: Focus on Temperature Uniformity

Poor temperature uniformity is rarely the result of one factor-many elements contribute to firing consistency. This column will focus on the heart of the kiln-the burner and combustion system.

Figure 1. Entrainment can eliminate localized overheating of the ware and furniture.

Burners

When the high-velocity style of burner was introduced over 30 years ago, it was quickly embraced as a means of achieving temperature consistency. The idea makes sense-a burner developing a stream of 400 mph gases must provide a great degree of circulation, and the ability to penetrate the load with convective gases does, indeed, improve uniformity.

A high-velocity stream of gases also has another important quality: the ability to induce or entrain internal kiln gases into the stream. This causes far greater degrees of circulation-as much as 10 times the burner stream volume. And very importantly, it also reduces the temperature of the gaseous stream. Consider the burner operating in Figure 1. Even though the burner jet is very hot (1700ºC), the actual jet temperature is only 1245ºC (with a kiln temperature of 1200ºC). Clearly, the entrainment has eliminated the chance for extremely hot areas of burner splash and severe, localized overheating of the ware and furniture.

But entrainment is only a part of the story. It is also critical that the burners be mounted correctly, and this is an area where many kiln manufacturers miss the boat. Most of the entrainment occurs right at the outlet of the burner block; if the block is recessed back into the wall, then entrainment is severely limited. Suddenly, the entrainment is only two or three times the jet volume, and the jet stream above becomes several hundred degrees hotter, resulting in hot spots in areas close to the burner.

When you examine any kiln design, always look at the outlet nozzle of the burner. It should be mounted even with the interior wall of the kiln-not recessed into a port or opening. Some burner manufacturers suggest the use of a venturi block to offset the problem, but this is no solution. The blocks don't significantly help entrainment, and even worse, they block the outlet of the burner when they fail.

Combustion Systems

If entrainment is a good thing, then the kiln's combustion system should be able to insure that it occurs. As you know, there are three primary types of combustion systems: proportional, excess air and pulse.

In proportional systems, air and fuel are proportioned at the proper ratio. Temperatures in the kiln (or zone) are maintained by increasing the air and fuel in tandem. This is a problem, however, because the degree of entrainment always varies. If the burner is at 100% output, the picture looks like Figure 1. When the burner is operating at 50% of output, however, the velocity of the burner is half as much, and the entrainment is halved too. The resulting jet stream of temperatures becomes 1283ºC-enough to make for some hot spots. As the burner throttles down further, the situation becomes worse. The only plus for proportional systems is that they are efficient-minimal or no excess air is used, and this saves fuel.

Excess air systems maintain the combustion air at a fixed level and throttle the fuel to maintain set point requirements. If the air is set at a high level, then all is well-the velocity emanating from the burner is high, entrainment approaches the 10x volume, and the combined jet stream is very close to ware temperature. This would be a great system, if fuel were inexpensive. But the reality is that typical excess air systems consume anywhere from 20-40% more fuel than proportional systems. This may be fine in some specialized applications, but it is not cost efficient in most cases.

Pulse firing is decidedly different, in that it applies nearly all of the required heat input with the burner at maximum firing rate, at stoichiometric ratio. To maintain temperature control, either the pulse high-fire time is varied (preferable), or the time between fixed duration pulses is varied. In this way, a properly designed pulse system always provides the maximum entrainment capability.

Did you enjoy this article? Click here to subscribe to Ceramic Industry Magazine.

Ralph-ruark-107px

Ralph Ruark is president of Swindell Dressler International. He was formerly president of Ruark Engineering, Inc., a company that provided analysis, recommendations and training for clients worldwide that manufacture industrial ceramics. He can be reached at (412) 788-7100 or rruark@swindelldressler.com.

Recent Articles by Ralph Ruark

You must login or register in order to post a comment.

Multimedia

Videos

Podcasts

Thermal Processing Optimization: Using Advanced Rotary Tube Internals

Mike Maggio of Harper International discusses rotary tube internals with Susan Sutton, editor-in-chief.

More Podcasts

THE MAGAZINE

Ceramic Industry Magazine

CI May 2013 cover

2013 May

The 2013 May Ceramic Industry includes articles on treating heat like light, recycling, solar energy, and more. Check it out today!

Table Of Contents Subscribe

THE CERAMIC INDUSTRY STORE

M:\General Shared\__AEC Store Katie Z\AEC Store\Images\Ceramics Industry\handbook of advanced ceramics.gif
Handbook of Advanced Ceramics Machining

Ceramics, with their unique properties and diverse applications, hold the potential to revolutionize many industries, including automotive and semiconductors.

More Products

Clear Seas Research

Clear Seas ResearchWith access to over one million professionals and more than 60 industry-specific publications,Clear Seas Research offers relevant insights from those who know your industry best. Let us customize a market research solution that exceeds your marketing goals.

Directories

0711ci_cover.gif

Ceramic Industry's Directories including Components, Equipment Digest, Services, Data Book & Buyers Guide, Materials Handbook and much more!

STAY CONNECTED

facebook_40px twitter_40px  youtube_40pxlinkedin_40