KILN CONNECTION: Fuel Conservation in a Slow Economy

Efficiency can be improved by making a few fundamental changes in the way a kiln is operated with reduced output. At a time when plants are struggling to achieve breakeven with low revenue, this technique can help brick manufacturers reduce fuel consumption.

Plants often have to curb the output of their kilns during economic slow-downs. This is no problem with periodic kilns, since they needn’t be fired as often and the fuel consumption in BTU/lb is normal. Continuous tunnel kilns do present challenges in efficiency when output is reduced, however.

We all know that the efficiency of tunnel kilns depends to a great extent on the cycle time of the ware processed. The fixed input to the kiln varies, but a reasonable value is around 50% of the fuel consumed at fast cycles. This fraction of the input doesn’t go away, even if the push cycle is slowed drastically. As a result, the input must be amortized over fewer and fewer pieces of ware, meaning the BTU/lb value increases significantly.

Efficiency can be improved, even at slower cycles, by making a few fundamental changes in the way the kiln is operated with reduced output. At a time when plants are struggling to achieve breakeven with low revenue, this technique can help brick manufacturers reduce fuel consumption.

Figure 1. Typical firing curve for a tunnel kiln firing face brick on a 24-hour cold-to-cold cycle.

Case in Point

As an example, consider a tunnel kiln that normally fires face brick on a rapid schedule of 24 hours cold-to-cold. Figure 1 illustrates a typical curve. In this cycle, the initial heating rate is around 140ºF/hour up to 1400ºF. Oxidation from 1400 to 1700ºF takes four hours, and 1700ºF to soak requires an additional four hours. Finally, the soaking time is an hour. Let’s assume that this is the fastest possible cycle.

When the kiln is slowed to half speed, the new cycle is 48 hours, and normally the only changes that are made would be to reduce the soaking temperature somewhat to maintain the proper brick absorption. There is nothing wrong with this method of operation, but knowing what the cycle must be to attain good properties allows for a different procedure that will save energy.

Figure 2. After reducing the preheating burners, the revised firing cycle (curve shown in red) for the same kiln closely matches the original while providing reduced fuel consumption.

Simple Adjustments

Since the optimum firing cycle is known, we can save a considerable amount of energy by reducing the preheating temperatures. Energy applied by the preheating burners is essential in fast cycles, but the burner gases in this part of the kiln can only pass through the load for a short time before the exhaust system removes them-and some of their energy-from the kiln.

We can turn off many of the preheating burners in our slow cycle and still stay below the heating maximum rates acceptable to the brick. This has the effect of reducing the exhaust temperature, therefore saving a significant amount of fuel. The new curve (in red) is shown in Figure 2.

Although the heating rates look different when drawn this way, they closely match the black curve that represents the standard cycle. The heating rates are similar for both curves, and the oxidation time is the same. The soaking temperature is slightly lower because we have twice as much time available at the depressed cycle. Most importantly, the fuel savings using this technique are significant.

When applying this technique, we need to be sure that we maintain the exhaust temperature at a level high enough to avoid condensation. We also need to keep an eye on heat uniformity to ensure that it doesn’t suffer too much without the benefit of preheat burner circulation. This viable technique will help reduce fuel consumption in times of decreased demand-which is just when we need to save as much money as possible. 

Links

Did you enjoy this article? Click here to subscribe to Ceramic Industry Magazine.

Ralph-ruark-107px

Ralph Ruark is president of Swindell Dressler International. He was formerly president of Ruark Engineering, Inc., a company that provided analysis, recommendations and training for clients worldwide that manufacture industrial ceramics. He can be reached at (412) 788-7100 or rruark@swindelldressler.com.

Recent Articles by Ralph Ruark

You must login or register in order to post a comment.

Multimedia

Videos

Podcasts

Improving HTCCs and LTCCs
Jim Ellis of Credence Engineering discusses the optimization of ceramic substrates for microelectronics applications.
More Podcasts

THE MAGAZINE

Ceramic Industry Magazine

CI June 2013 cover

2013 June

The 2013 June Ceramic Industry includes articles on flat boron, decorative tile, patents, OLED lighting, and more. Check it out today!

Table Of Contents Subscribe

THE CERAMIC INDUSTRY STORE

M:\General Shared\__AEC Store Katie Z\AEC Store\Images\Ceramics Industry\handbook of advanced ceramics.gif
Handbook of Advanced Ceramics Machining

Ceramics, with their unique properties and diverse applications, hold the potential to revolutionize many industries, including automotive and semiconductors.

More Products

Clear Seas Research

Clear Seas ResearchWith access to over one million professionals and more than 60 industry-specific publications,Clear Seas Research offers relevant insights from those who know your industry best. Let us customize a market research solution that exceeds your marketing goals.

Directories

0711ci_cover.gif

Ceramic Industry's Directories including Components, Equipment Digest, Services, Data Book & Buyers Guide, Materials Handbook and much more!

STAY CONNECTED

facebook_40px twitter_40px  youtube_40pxlinkedin_40