“The 2500 Kyocera KC200 modules are performing at 105% of expected output after nearly three years of operation,” said Steve Gabrielle, PPL Renewable Energy’s director. “Each year, this system is producing about 30,000 kilowatt hours (kWh) more than planned.”
In total, the installation produces 630,000 kWh annually, enough to power 72 typical area homes while offsetting 198 metric tons of carbon dioxide emissions-the equivalent of taking 36 cars off the road and saving 900 barrels of oil each year.
“We’re very pleased that our collaboration with Kyocera resulted in an installation that is over-performing,” said Gabrielle. “That’s great news for PPL, its energy customers and the state of New Jersey. This partnership is an example of PPL’s commitment to renewable energy options in cultivating the next generation of power.”
“Kyocera is committed to environmental preservation and providing quality solar energy solutions to the world,” said Chris Brown, sales manager for Kyocera Solar. “For this reason, we are pleased to have Kyocera’s solar modules utilized as one of the key technologies demonstrated in the PPL Renewable Energy Park.”
For more information, visit www.kyocerasolar.com.