Magneco/Matrel: Nanotechnology For Furnaces

March 28, 2005
/ Print / Reprints /
ShareMore
/ Text Size+
Magneco/Metrel, Inc. recently announced that its spray-on nanoparticulate refractory, known as Met-Silcast(TM), is now available for furnace construction and repair in the glass, petrochemical and copper industries. "An original development of Magneco/Metrel, this is advanced refractory technology with time-tested and important new benefits," said Charles W. Connors, Sr., chief executive officer. "Its impact has been revolutionary because it can be applied in hours, instead of weeks or months, to create a low-cost, endlessly renewable furnace lining that improves end-product quality and operational performance, while dramatically reducing downtime as well as construction and maintenance costs." Met-Silcast consists of a pumpable, colloidal silica-bonded, monolithic refractory material that offers many advantages over traditional brick refractory.

For additional information, call (630) 543-6660 or visit http://www.magneco-metrel.com.

Did you enjoy this article? Click here to subscribe to Ceramic Industry Magazine.

You must login or register in order to post a comment.

Multimedia

Videos

Image Galleries

April 2014 Issue Highlights

Our April 2014 issue is now available!

Podcasts

Sapphire: An Extreme Performer

Ian Doggett of Goodfellow and CI Editor Susan Sutton discuss the benefits and opportunities provided by industrial sapphire.

More Podcasts

Ceramic Industry Magazine

CI August 2014 cover

2014 August

Explore technical ceramics, glasses and refractories in our August issue!

Table Of Contents Subscribe

THE CERAMIC INDUSTRY STORE

M:\General Shared\__AEC Store Katie Z\AEC Store\Images\Ceramics Industry\handbook of advanced ceramics.gif
Handbook of Advanced Ceramics Machining

Ceramics, with their unique properties and diverse applications, hold the potential to revolutionize many industries, including automotive and semiconductors.

More Products

Clear Seas Research

Clear Seas ResearchWith access to over one million professionals and more than 60 industry-specific publications,Clear Seas Research offers relevant insights from those who know your industry best. Let us customize a market research solution that exceeds your marketing goals.

Directories

CI Data Book July 2012

Ceramic Industry's Directories including Components, Equipment Digest, Services, Data Book & Buyers Guide, Materials Handbook and much more!

STAY CONNECTED

facebook_40px twitter_40px  youtube_40pxlinkedin_40google+ icon 40px