Magnesium Oxide Output Expected to Remain Depressed (posted 10/19/09)

According to a new report, it could be 2011-2012 before magnesium oxide sales volumes rebound to 2005-2007 tonnage levels.

According to a new report from MarketPublishers entitled “Magnesium Oxide (MgO) Market Research Report 2009,” in 2008, many magnesium oxide manufacturers announced plans for production volume growth, new plant construction, and diversification, as well as the output resumption of earlier produced MgO grades. However, in 2009, the output of magnesium oxide has declined dramatically due to a reduction in demand. According to the report, it could be 2011-2012 before magnesium oxide sales volumes rebound to 2005-2007 tonnage levels.

Magnesium oxide is used mainly as a refractory material in furnace linings for producing iron and steel, nonferrous metals, glass, and cement. Visit www.marketpublishers.com for additional details.

Links

Did you enjoy this article? Click here to subscribe to Ceramic Industry Magazine.

You must login or register in order to post a comment.

Multimedia

Videos

Podcasts

Thermal Processing Optimization: Using Advanced Rotary Tube Internals

Mike Maggio of Harper International discusses rotary tube internals with Susan Sutton, editor-in-chief.

More Podcasts

THE MAGAZINE

Ceramic Industry Magazine

CI May 2013 cover

2013 May

The 2013 May Ceramic Industry includes articles on treating heat like light, recycling, solar energy, and more. Check it out today!

Table Of Contents Subscribe

THE CERAMIC INDUSTRY STORE

M:\General Shared\__AEC Store Katie Z\AEC Store\Images\Ceramics Industry\handbook of advanced ceramics.gif
Handbook of Advanced Ceramics Machining

Ceramics, with their unique properties and diverse applications, hold the potential to revolutionize many industries, including automotive and semiconductors.

More Products

Clear Seas Research

Clear Seas ResearchWith access to over one million professionals and more than 60 industry-specific publications,Clear Seas Research offers relevant insights from those who know your industry best. Let us customize a market research solution that exceeds your marketing goals.

Directories

0711ci_cover.gif

Ceramic Industry's Directories including Components, Equipment Digest, Services, Data Book & Buyers Guide, Materials Handbook and much more!

STAY CONNECTED

facebook_40px twitter_40px  youtube_40pxlinkedin_40