MATERIAL INNOVATIONS: Holding a Charge

Newly discovered titanium nitride-based superinsulators promise to transform materials research and electronics design.

To perform the experiment, researchers used a dilution refrigerator, a device in which the temperature can be lowered to several millikelvin, just above absolute zero.


Superinsulation is a newly discovered fundamental state of matter created by scientists at the U.S. Department of Energy’s Argonne National Laboratory in collaboration with several European institutions. Led by Argonne senior scientist Valerii Vinokur and Russian scientist Tatyana Baturina, an international team of scientists from Argonne, Germany, Russia and Belgium fashioned a thin film of titanium nitride that they then chilled to near absolute zero.

When they tried to pass a current through the material, the researchers noticed that the material’s resistance suddenly increased by a factor of 100,000 once the temperature dropped below a certain threshold. The same sudden change also occurred when the researchers decreased the external magnetic field.

Possible Applications

Like superconductors, which have applications in many different areas of physics (from accelerators and magnetic-levitation trains to MRI machines), superinsulators could eventually find their way into a number of products, including circuits, sensors and battery shields. For example, if a battery is left exposed to the air, the charge will eventually drain from it in a matter of days or weeks because the air is not a perfect insulator, according to Vinokur. “If you pass a current through a superconductor, it will carry the current forever. Conversely, if you have a superinsulator, it will hold a charge forever,” he said.

“Titanium nitride films, as well as films prepared from some other materials, can be either superconductors or insulators depending on the thickness of the film,” Vinokur said. “If you take the film, which is just on the insulating side of the transition, and decrease the temperature or magnetic field, then the film all of a sudden becomes a superinsulator.”

Scientists could eventually form superinsulators that would encapsulate superconducting wires, creating an optimally efficient electrical pathway with almost no energy lost as heat. A miniature version of these superinsulated superconducting wires could find its way into more efficient electrical circuits.

Argonne scientist Valerii Vinokur and Russian collaborator Tatyana Baturina examine a graph of the resistance of the insulating film plotted against the applied magnetic field.

How Does it Work?

Titanium nitride’s sudden transition to a superinsulator occurs because the electrons in the material join together in twosomes called Cooper pairs. When these Cooper pairs of electrons join together in long chains, they enable the unrestricted motion of electrons and the easy flow of current, creating a superconductor. In superinsulators, however, the Cooper pairs stay separate from each other, forming self-locking roadblocks.

“In superinsulators, Cooper pairs avoid each other, creating enormous electric forces that oppose the penetration of the current into the material,” said Vinokur. “It’s exactly the opposite of the superconductor.”

The theory behind the experiment stemmed from Argonne’s Materials Theory Institute (MTI), which Vinokur organized six years ago in the laboratory’s Materials Science Division. The MTI hosts a handful of visiting scholars from around the world to perform cutting-edge research on the most pressing questions in condensed matter physics. Upon completion of their tenure at Argonne, these scientists return to their home institutions but continue to collaborate on the joint projects. The MTI attracts the world’s best condensed matter scientists, including Russian Tatyana Baturina, who, according to Vinokur, “became a driving force in our work on superinsulators.”

Scientists from the Institute of Semiconductor Physics in Novosibirsk, Russia, Regensburg and Bochum universities in Germany and the Interuniversity Microelectronics Centre in Leuven, Belgium, also participated in the research.

Funding for this experiment came principally from the Novosibirsk Institute of Semiconductor Physics and the University of Regensberg. The Basic Energy Sciences Division of the Department of Energy’s Office of Science and Argonne Materials Theory Institute also contributed in part to the research, which appears in the April 3 issue of Nature. Visit www.anl.gov for more information.

Links

Did you enjoy this article? Click here to subscribe to Ceramic Industry Magazine.

You must login or register in order to post a comment.

Multimedia

Videos

Podcasts

Thermal Processing Optimization: Using Advanced Rotary Tube Internals

Mike Maggio of Harper International discusses rotary tube internals with Susan Sutton, editor-in-chief.

More Podcasts

THE MAGAZINE

Ceramic Industry Magazine

CI May 2013 cover

2013 May

The 2013 May Ceramic Industry includes articles on treating heat like light, recycling, solar energy, and more. Check it out today!

Table Of Contents Subscribe

THE CERAMIC INDUSTRY STORE

M:\General Shared\__AEC Store Katie Z\AEC Store\Images\Ceramics Industry\handbook of advanced ceramics.gif
Handbook of Advanced Ceramics Machining

Ceramics, with their unique properties and diverse applications, hold the potential to revolutionize many industries, including automotive and semiconductors.

More Products

Clear Seas Research

Clear Seas ResearchWith access to over one million professionals and more than 60 industry-specific publications,Clear Seas Research offers relevant insights from those who know your industry best. Let us customize a market research solution that exceeds your marketing goals.

Directories

0711ci_cover.gif

Ceramic Industry's Directories including Components, Equipment Digest, Services, Data Book & Buyers Guide, Materials Handbook and much more!

STAY CONNECTED

facebook_40px twitter_40px  youtube_40pxlinkedin_40