New Products / Product Highlights

Meller Optics, Inc.: Optical Lapping Pitch (posted 7/10/08)

The petroleum-free optical lapping pitch is available in five grades from very-soft to very-hard, with melting points from 52 to 87°C.

A line of petroleum-free optical lapping pitch that helps to maintain the purity of the polishing media and substrate is available from Meller Optics, Inc. Meller Gugolz optical lapping pitch is made from all-natural wood resin, which helps prevent contamination of the polishing media and substrates. Featuring five grades from very-soft to very-hard, with melting points from 52 to 87°C, users can simply slice the amount required, melt it and pour the lap.

Ready to use without screening, filtering or mixing additives, Meller Gugolz optical lapping pitch is ideally suited for blocking, lapping and polishing applications. All five hardness grades are fully compatible, allowing users to achieve any intermediate grade of hardness.

For more information, call (800) 821-0180, fax (401) 331-0519, e-mail steve@melleroptics.com or visit www.melleroptics.com.

Links

Did you enjoy this article? Click here to subscribe to Ceramic Industry Magazine.

You must login or register in order to post a comment.

Multimedia

Videos

Podcasts

Thermal Processing Optimization: Using Advanced Rotary Tube Internals

Mike Maggio of Harper International discusses rotary tube internals with Susan Sutton, editor-in-chief.

More Podcasts

THE MAGAZINE

Ceramic Industry Magazine

CI May 2013 cover

2013 May

The 2013 May Ceramic Industry includes articles on treating heat like light, recycling, solar energy, and more. Check it out today!

Table Of Contents Subscribe

THE CERAMIC INDUSTRY STORE

M:\General Shared\__AEC Store Katie Z\AEC Store\Images\Ceramics Industry\handbook of advanced ceramics.gif
Handbook of Advanced Ceramics Machining

Ceramics, with their unique properties and diverse applications, hold the potential to revolutionize many industries, including automotive and semiconductors.

More Products

Clear Seas Research

Clear Seas ResearchWith access to over one million professionals and more than 60 industry-specific publications,Clear Seas Research offers relevant insights from those who know your industry best. Let us customize a market research solution that exceeds your marketing goals.

Directories

0711ci_cover.gif

Ceramic Industry's Directories including Components, Equipment Digest, Services, Data Book & Buyers Guide, Materials Handbook and much more!

STAY CONNECTED

facebook_40px twitter_40px  youtube_40pxlinkedin_40