Mofratech Offers New Aluminum Surface Coating Process

Mofratech recently introduced its Altim TD® process for the transformation of the surface of aluminum into a hard, thick ceramic layer. Unlike many other anodizing or electrolytic coating methods, the new process is reportedly pollution free and is in full compliance with current and proposed environmental regulations worldwide. According to the company, the coating, which consists of a micro-arc oxidation process that is primarily of the alpha-alumina (corundum) phase of aluminum oxide, offers a hardness of 1,400 to 2,000 HV and wear resistance four times as great as conventional hard- anodized aluminum.

For additional information, call (33) 4 50 33 70 22, fax (33) 4 50 33 70 26, e-mail mofra@dial.oleane.com or visit http://www.mofratech.com.

Did you enjoy this article? Click here to subscribe to Ceramic Industry Magazine.

You must login or register in order to post a comment.

Multimedia

Videos

Podcasts

Thermal Processing Optimization: Using Advanced Rotary Tube Internals

Mike Maggio of Harper International discusses rotary tube internals with Susan Sutton, editor-in-chief.

More Podcasts

THE MAGAZINE

Ceramic Industry Magazine

CI May 2013 cover

2013 May

The 2013 May Ceramic Industry includes articles on treating heat like light, recycling, solar energy, and more. Check it out today!

Table Of Contents Subscribe

THE CERAMIC INDUSTRY STORE

M:\General Shared\__AEC Store Katie Z\AEC Store\Images\Ceramics Industry\handbook of advanced ceramics.gif
Handbook of Advanced Ceramics Machining

Ceramics, with their unique properties and diverse applications, hold the potential to revolutionize many industries, including automotive and semiconductors.

More Products

Clear Seas Research

Clear Seas ResearchWith access to over one million professionals and more than 60 industry-specific publications,Clear Seas Research offers relevant insights from those who know your industry best. Let us customize a market research solution that exceeds your marketing goals.

Directories

0711ci_cover.gif

Ceramic Industry's Directories including Components, Equipment Digest, Services, Data Book & Buyers Guide, Materials Handbook and much more!

STAY CONNECTED

facebook_40px twitter_40px  youtube_40pxlinkedin_40