Ceramic Industry News

NREL Discovers Quantum Effect in Silicon Nanocrystals (posted 8/6/07)

Researchers at the U.S. Department of Energy’s National Renewable Energy Laboratory (NREL) have shown that a new effect called multiple exciton generation occurs efficiently in silicon nanocrystals.

Researchers at the U.S. Department of Energy’s National Renewable Energy Laboratory (NREL), collaborating with Innovalight, Inc., have shown that a new and important effect called multiple exciton generation (MEG) occurs efficiently in silicon nanocrystals. MEG results in the formation of more than one electron per absorbed photon.

Silicon is the dominant semiconductor material used in present day solar cells, representing more than 93% of the photovoltaic cell market. Until this discovery, MEG had been reported over the past two years to occur only in nanocrystals (also called quantum dots) of semiconductor materials that are not presently used in commercial solar cells, and which contain environmentally harmful materials (such as lead). The new result opens the door to the potential application of MEG for greatly enhancing the conversion efficiency of solar cells based on silicon because more of the sun’s energy is converted to electricity. This is a key step toward making solar energy more cost-competitive with conventional power sources.

In a paper published on July 24 in the initial online version of the American Chemical Society’s “Nano Letters Journal,” a NREL team reported that silicon nanocrystals, or quantum dots, obtained from Innovalight can produce more than one electron from single photons of sunlight that have wavelengths less than 420 nm. When today’s photovoltaic solar cells absorb a photon of sunlight, about 50% of the incident energy is lost as heat. MEG provides a way to convert some of this energy lost as heat into additional electricity.

The silicon nanocrystals produced by Innovalight, a thin-film solar cell developer based in Santa Clara, Calif., were studied at NREL as part of a collaboration between NREL and Innovalight scientists. The NREL team consisted of Matthew C. Beard, Kelly P. Knutsen, Joseph M. Luther, Qing Song, Wyatt Metzger, Randy J. Ellingson and Arthur J. Nozik.

The findings represent an important extension of the range of semiconductor materials that exhibit MEG and are a further confirmation of pioneering work by Nozik, who in 1997 predicted that semiconductor quantum dots could exhibit efficient electron multiplication and hence increase the efficiency of solar cells.

To date, all experiments showing the production of more than one electron per absorbed photon have been based on various types of optical spectroscopy. In a solar cell device, it is necessary to extract the electrons produced in the quantum dots and pass them through an external circuit to generate electrical power. Such experiments are currently underway at NREL, Innovalight and other laboratories to demonstrate that MEG can indeed lead to enhanced solar cell efficiencies.

Calculations at NREL by Mark Hanna and Nozik have shown that the maximum theoretical efficiency of quantum dot solar cells exhibiting optimal MEG is about 44% with normal unconcentrated sunlight and 68% with sunlight concentrated by a factor of 500 with special lenses or mirrors. Today’s conventional solar cells that produce one electron per photon have maximum efficiencies of 33% and 40%, respectively, under the same solar conditions.

In addition to efficiently extracting the electrons from the quantum dots in solar cells, future research is directed toward producing MEG at wavelengths that have a greater overlap with the solar spectrum, as well as producing a much sharper onset of the MEG processes with decreasing wavelength of the photons.

For more information, call (303) 275-4090 or visit www.nrel.gov. Innovalight’s website is located at www.innovalight.com.

Links

Did you enjoy this article? Click here to subscribe to Ceramic Industry Magazine.

You must login or register in order to post a comment.

Multimedia

Videos

Podcasts

Thermal Processing Optimization: Using Advanced Rotary Tube Internals

Mike Maggio of Harper International discusses rotary tube internals with Susan Sutton, editor-in-chief.

More Podcasts

THE MAGAZINE

Ceramic Industry Magazine

CI May 2013 cover

2013 May

The 2013 May Ceramic Industry includes articles on treating heat like light, recycling, solar energy, and more. Check it out today!

Table Of Contents Subscribe

THE CERAMIC INDUSTRY STORE

M:\General Shared\__AEC Store Katie Z\AEC Store\Images\Ceramics Industry\handbook of advanced ceramics.gif
Handbook of Advanced Ceramics Machining

Ceramics, with their unique properties and diverse applications, hold the potential to revolutionize many industries, including automotive and semiconductors.

More Products

Clear Seas Research

Clear Seas ResearchWith access to over one million professionals and more than 60 industry-specific publications,Clear Seas Research offers relevant insights from those who know your industry best. Let us customize a market research solution that exceeds your marketing goals.

Directories

0711ci_cover.gif

Ceramic Industry's Directories including Components, Equipment Digest, Services, Data Book & Buyers Guide, Materials Handbook and much more!

STAY CONNECTED

facebook_40px twitter_40px  youtube_40pxlinkedin_40