The new Krautkramer CL 400 precision thickness gauge introduced by Agfa NDT offers advancements in ultrasonic performance and straightforward operation. In addition, instrument capabilities can be extended with optional A-Scan and programmable data recorder features. Fast readings minimize test times while stability increases confidence in measurement accuracy. The high degree of performance is the result of combining advanced signal processing with a large selection of compatible, highly damped single element transducers.
For more information, call (717) 242-0327, ext. 223.