Airguard has developed Stackguard(R), a paint arrestor media that is 99%+ efficient for a wide range of paints, coatings and glazes. Stackguard incorporates fiber glass media for high paint holding capacity with a polyester backing for high particulate efficiency. This high-performing collection media holds 35 times its weight in paint particulate overspray -- and has a tensile strength three times higher than paper-backed medias, per ASTM #D-1682. The 2-in. Stackguard offers a clean resistance to airflow of .02 at 100 fpm or .30 at 500 fpm, while the 4-in. version has a clean resistance to aiflow of .05 at 100 fpm and .52 at 500 fpm. Both are sold in rolls or pads, in widths from 20 to 60 in.
For more information, call (800) 999-3458, fax (502) 961-0930 or visit http://www.airguard.com.