Aremco Products, Inc.'s new Ceramabond(TM) 690 is a single-part, boron nitride-filled ceramic adhesive and coating system for use in oxidizing atmospheres to 1560F and reducing and vacuum environments to 2700F. This system offers high thermal conductivity of 55 W/m-K, high dielectric strength of 500 volts/mil, and exceptional resistance to molten glasses and metals. Ceramabond 690 is formulated with a phosphate binder that provides excellent adhesive strength in bonding applications. Applications are found in the metals and glass industries for insulating molds, dies and other structures from attack by molten metals, salts and glasses.