Ceramacast(TM) 510 from Aremco Products, Inc. is an aluminum oxide-based, hydraulic-setting ceramic compound ideal for encapsulating cartridge heaters and embedding high temperature components such as induction heating coils to 3200F (1760C). Ceramacast 510 is supplied as a dry powder, formulated with a high alumina content of greater than 90%. It is bonded using calcium aluminate, and the "as-cast" and dried density is 180 lbs/ft(3). Exceptional thermal conductivity and a high dielectric strength of 75-100 volts/mil are provided. Ceramacast 510 is mixed with water to a paste-like consistency in a ratio of 100 parts powder to 15-19 parts water. It provides one hour pot life and hardening time of five hours. Full cure is achieved after drying at room temperature for 24 hours.
For more information, call (845) 268-0039, fax (845) 268-0041, e-mail aremco@aremco.com or visit http://www.aremco.com.