Ultra-Temp
TM 516, a new single part, zirconia-filled, inorganic adhesive system from Aremco Products, Inc., is available for bonding zirconia components in high temperature sensors and instruments to 4400F. Ultra-Temp 516 demonstrates exceptional electrical, mechanical and thermal properties, including dielectric strength of 250 volts/mil, volume resistivity of 10(8) ohm-cm and torque strength of 8.6 in-lbs. Due to its inert chemistry, the adhesive will not outgas under ultra-high vacuum. It also provides excellent chemical, moisture and thermal shock resistance.