Blasch Precision Ceramics' new InVinCer™ lines of high-performance advanced silicon carbide products have been introduced to several market segments. Blasch's new reaction bonded material, SiSiC, offers excellent wear, chemical, oxidation and thermal shock resistance, as well as the highest thermal conductivity to its maximum use temperature of 1380°C. Available products include rollers, beams, posts, burner nozzles, pump components, crucibles, mechanical seals, micronizers, cyclones and sand blasting nozzles. Custom shapes are also available upon request. The Blasch product introduction is targeted for the sanitaryware, tableware, technical, porcelain, refractory ceramic and artware/hobbyist market segments.
For additional information, call (800) 550-5768 or (518) 436-1263, ext. 45; fax (518) 436-0098; e-mail skubiak@blaschceramics.com; or visit link below.
Links