According to "RGB-041Y Powder Metallurgy," an updated report from Business Communications Co., Inc. (BCC), the North American metal powder market was estimated at 1.14 billion pounds, worth $2.4 billion, in 2003 and is forecast to reach 1.45 billion pounds, worth $3.4 billion, in 2008. The P/M parts market was estimated at 993 million pounds, worth $5.4 billion, in 2003 and is forecast to reach nearly 1.3 billion pounds, worth about $7.7 billion, in 2008.