Centorr Vacuum Industries has shipped one of its Series LF furnace systems to a major university in the People’s Republic of China. This high-temperature (2000°C), high-vacuum (10-6 torr) furnace system features a long-life, ultra-clean tungsten heating element and a hot zone diameter of 76 x 127 mm high. The system also has a programmable controller with RS communication capability.
The LF line of furnaces is available with rough pumping, diffusion pumping and turbo-molecular pumping systems. All of the furnaces are capable of heating in inert gas and are ready for immediate shipment.