Ceramic Industry

Ceramic Services Supplies Drying System For Saxonburg Ceramics

May 16, 2005
Saxonburg Ceramics, Monroe, N.C., recently placed a new drying system into production. Ceramic Services Inc. was contracted to completely design, build and install this environmentally controlled batch dryer. The new system is a three cart, positive pressure system, providing programmable control for air, temperature and humidity. The installation of these upgrades has resulted in greatly improved drying time and lowered scrap of Saxonburg's product.

For more information on Saxonburg Ceramics, visit http://www.saxonburgceramics.com. Ceramic Services' website is located at http://www.kilnman.com.