According to “Boron: Global Industry Markets and Outlook,” from Roskill Information Services Ltd., the global demand for boron grew strongly in the three years to 2008. Products containing boron in the form of borates or boric acid pervade every part of everyday life, from borosilicate glass in LCD screens to composites used in car body panels and glass wool for loft insulation.
Growth has been driven by an expansion of demand from China, where consumption rose by 15% per year from 2000 to 2008. The increase in market share held by Asian countries reflects the shift in the production of textile-grade fiber glass, borosilicate glass, and ceramics away from North America and Europe to countries with lower production costs.
Following the years of strong growth, 2009 saw a sharp drop in demand for borates, but, in the second half of the year, markets for both textile-grade fiber glass and borosilicate glass recovered; demand for borosilicate glass in LCD screens is expected to grow by 15% in 2010. The main factors affecting future demand for textile-grade fiber glass are continued growth in electronic products, increased penetration of fiber glass in markets traditionally held by steel and concrete, and the emergence of new markets such as turbine blades for wind power generation. An up-turn in construction activity and the increase in government–led initiatives to reduce energy consumption will provide a recovering market for insulation-grade fiber glass in the medium-term.
World production of natural and refined borates remains highly concentrated in Turkey and the U.S., with Rio Tinto Minerals and Eti Mine accounting for around 75% of supply. The high B2O3 content (> 26%) of the colemanite, tincal and kernite mined in Turkey and California is the main factor contributing to the leading position of these two companies in world borates supply.
The gap between China’s domestic production and demand (and the relatively low-grade locally mined borates) has been, and will continue to be, the main factor driving capacity expansions worldwide. Since 2003, expansions undertaken by Rio Tinto Minerals in the U.S., Quiborax in Chile, Eti Mine in Turkey and Manufacturas Los Andes in Argentina have raised boric acid capacity by over 200,000 tons per year and were mainly aimed at the Chinese market.
Future expansion is dominated by plans to expand capacity for refined borates, boron oxide and calcined tincal in Turkey. Other projects under consideration are to increase boric acid production in Argentina and Bolivia and to exploit brine deposits in Tibet and Qinghai. In addition, Rio Tinto Minerals has plans to exploit the Jadar lithium borate deposit in Serbia.
For more information, call (44) 208944-0066, fax (44) 208947-9568, e-mail
info@roskill.co.uk or visit
www.roskill.com.