CILAS U.S., Inc. recently announced the availability of new literature detailing the features and benefits of its model 920 laser diffraction particle size analyzer. The new two-page, color brochure describes the analyzer, which is designed for measurements from 0.3 to 400 microns. An easy-to-use, Windows(TM)-compatible software package, The Particle Expert, provides for instrument operation, data processing and report generation. The 920 is available in liquid or dry dispersion configurations, as well as the company's patented "2 in 1 design," which offers the ability to change modes with a "click of a mouse."