CM Furnaces Inc. recently introduced its new high-performance, low-cost model 1704FL laboratory furnace. The newest addition to the popular CM line of rapid temperature furnaces is equipped with contemporary, technologically superior features and constructed of the highest caliber materials. Manufactured with a convenient 110-volt power supply and standard outlet plug, the model 1704FL furnace is user-friendly, installing in only minutes. Rated to operate continuously at 1700C, this furnace uses high-purity alumina fiber and Kanthal Super(R) 1800 molydisilicide heating elements, assuring rapid heat up and cool down rates. The 4 x 4 x 4-in. heated chamber is appropriately sized to accommodate most laboratory applications.