The new Meinzer II sieve shaker from CSC Scientific allows users to determine particle size easily and accurately for products ranging from 3 in. to 75 um in a matter of minutes. New technology provides an exacting sieve motion to give particles optimal time over the apertures of the sieves for precise, repeatable results. The Meinzer II is used to make this maintenance-free shaker an important asset for users' testing processes in various applications.