Datapaq recently announced the availability of its Kiln Tracker RF telemetry system, a real-time profiling system for monitoring temperatures during the firing process. This system is especially useful to brick and sanitaryware manufacturers that could be experiencing firing problems with a particular kiln profiling batch. Although kiln cars can be carefully monitored using a conventional kiln profiling system, the problem is not identified until the process is completed. Telemetry profiling provides the ability to see precisely what is happening to the ware during the firing process and to adjust the kiln settings while the batch is still in the kiln.