Devcon offers a full range of epoxy and urethane potting compounds and encapsulants with superior flexibility and impact and environmental resistance. Available in low- and non-shrink formulations, these compounds cure quickly at room temperature with minimal air entrapment. Flexane(R) compounds are castable, non-shrinking, two-component liquid urethanes that are easily mixed and poured. After curing at room temperature, they exhibit superior elasticity and flexibility. Flexane 80 liquid is a medium-viscosity (10,000 cps) compound that cures to a semi-rigid rubber material and will return to its original shape even after 650% elongation. It has a demolding time of 10 hours.