Hindustan Sanitaryware Achieves ISO 14001 Certification

December 4, 2000
Hindustan Sanitaryware & Inds. Ltd., Haryana, India, has achieved ISO 14001 certification. According to the company, it is the first sanitaryware company in India to achieve this certification.