These cover plates are designed to cover the investment mold during the preheat process to avoid possible contamination problems.
Industrial Ceramic Products, Inc.
This company's cover plates are designed to cover the investment mold during the preheat process to avoid possible contamination problems. These products reportedly withstand thermal shock at high temperatures and are compatible with pour cups and shell materials. They can be produced from the company's mullite or FUSIL 2000 materials.