The 5000 series, Lucifer Furnaces, Inc.'s line of large, heavy-duty electric production furnaces, is described in a new four-page brochure. The brochure includes information on the company's normal air models, atmosphere furnaces designed with alloy muffles, removable alloy muffles, elevator quench models, and atmosphere furnaces constructed with a gas-tight shell. The standard air models are available with chamber dimensions up to 48 x 48 x 72 in. and operation to 2300F. The company's alloy muffle furnaces offer a cost-effective means of providing scale-free heat treating with atmosphere. The brochure details general construction features; available options; and detailed specification charts, including chamber dimensions, overall sizes, power requirements and weights for each model.
For additional information, call (800) 378-0095, fax (215) 343-7388, e-mail info@luciferfurnaces.com or visit http://www.luciferfurnaces.com .