Lucifer Furnaces, Inc.'s line of protective atmosphere elevator quench furnaces is described in a four-page brochure. Bulletin 7000 provides complete specifications, dimensions and work load capacities for these furnaces, which are ideal for low-production, scale-free applications. Designed for 2100F operation, the units combine pre-heat selection, a hardening chamber, a cooling vestibule and a quench tank in one integrated unit. The furnaces are available in eight standard sizes, ranging in chamber size from 5 x 5 x 12 in. to 10 x 10 x 36 in. and workload capacity from 15 to 55 lbs. Options include equipment for fully-automated operation, safety equipment for combustible atmosphere operation, pusher rod assembly, air-operated doors, fan- or water-cooled vestibule, quench tank agitation and heating, sight ports, flow meter and regulator.