Lucifer Furnaces, Inc.'s line of gas-tight protective atmosphere furnaces, a low-cost alternative to retort-equipped furnaces, is described in a two-color brochure. The GT models combine a continuously welded heavy gauge sheet steel shell with a gasketed door assembly to provide a positive seal for either inert or flammable/combustible atmospheres. GT units are particularly cost-effective in facilities where heat treating in protective atmosphere is performed continuously. The brochure describes construction features, available options and benefits. Also included is a specification chart that details overall size, chamber size, power requirements and weight for each of the eight bench and eight floor models in the series.
For additional information, call (800) 378-0095, fax (215) 343-7388 or visit http://www.luciferfurnaces.com .