Ceramic Industry

Malvern and Hosokawa Develop Intelligent Milling System

August 19, 2002
Malvern Instruments and Hosokawa Micron have joined forces to develop Intellimill, a highly advanced intelligent milling system. The new unit integrates the Malvern Insitec on-line particle sizer into a range of process equipment, including air classifier mills and air jet mills. Intellimill will be launched at Powtech, October 8-10, Nurnberg, Germany. Information will be available at the Malvern stand (11-117), and Intellimill will be shown at the Hosokawa stand (7-437).