A unique two-component, room temperature curing, high-temperature resistant epoxy adhesive called EP35 has been introduced by Master Bond Inc. This system produces high-strength bonds that maintain strength even after long exposures to temperatures in the 450-500F range. It has a 100 to 70 mix ratio by weight and can be applied without sagging or dripping, even on vertical surfaces. Master Bond EP35 produces durable and tough bonds that are resistant to thermal cycling and chemicals including water, oil and most organic solvents. It offers adhesion to metals, glass, ceramics, wood, vulcanized rubbers and many plastics.