Ceramic Industry

Matec Applied Sciences: Particle Sizer Patent

April 22, 2003
Matec Applied Sciences has been granted a patent for a new device called the APS (acoustic particle sizer), which is capable of simultaneously measuring -- without the need for prior sample dilution -- particle size distribution (PSD), percent solids, acoustic attenuation and sound speed spectra, pH, temperature, and conductivity of numerous types of colloids. The APS will replace traditional light scattering-based instruments that require high sample pre-dilution, which can change the dispersion's PSD and introduce operator error. The APS will also be used as a process on-line and QC device thanks to its ability to characterize undiluted samples. The APS uses a patented particle size algorithm developed by Lucent Technologies.

For more information, call (508) 393-0155, e-mail colloid@matec.com or visit http://www.matec.com .