Minox, GmbH recently introduced a new line of air-jet sieves called the Air-Jet MLS 200. These machines are used to test dry materials of all kinds from 20-1000 microns. The units can analyze sample quantities between 1-200 grams without the degrading effects associated with other mechanical shaking units. Both the negative and positive pressure can be adjusted with the use of manual control wheels, making it possible to reproduce any test with exact conditions. Users can use standard test sieves in either 8-in. or 200-mm sizes from their existing lab stock, which eliminates the need for expensive custom test sieves.