A 36-page directory from the Metal Powder Industries Federation
(MPIF) provides information on sources of 87 ferrous and nonferrous
metal powders, including refractory metals such as tungsten,
tantalum, cobalt, molybdenum and niobium. The directory provides
detailed product information from members of the Metal Powder
Producers Association and the Refractory Metals Association.
Information is given on commercially available powders, special
powders and manufacturing capabilities of leading North American
companies.